I have recently taken delivery of an XF sportwagon and decided to fit mudflaps.
To my horror, I find that there is a strip of foam between the inner and outer sills for the whole length and this causes me concern for the future.
Has anyone any experience of how this might effect the inner sill as time passes by?
Obviously my concern is rust.
Foam between outer and inner sills
Moderator:cawthrm
- raysearles

- Posts:397
- Joined:Fri Mar 12, 2010 6:47 pm
Re: Foam between outer and inner sills
Speak to the guys at XJK our technical experts, I am sure they will have a view that can help
-
ianoliver57

- Posts:261
- Joined:Fri Mar 14, 2014 11:19 pm
- Location:Tayvallich, Argyll.
Re: Foam between outer and inner sills
Was this ever resolved? I was changing to my winter wheels yesterday and discovered a square 'hole' below the sill just beside the jacking point which had wet foam inside. What is this for? Can it be removed? Presumably Jaguar cars put it there for a specific reason but I cannot see what at the moment.
Any thoughts?
Any thoughts?
2009 XJ8 Sovereign X358 Final Edition 4.2 V8.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Re: Foam between outer and inner sills
Those of us more familiar with the S type model are only too well aware of corrosion beneath the plastic over sill. As conformation of this look at the list of S type Mot failures for sale on E bay together with copious amounts of copy and pictures on this subject on the S type section.
I suspect that the construction of the XF in the sill area is identical to that of the S type and for that reason I would have the plastic over sills off and remove the foam insert. While at it,do not miss the opportunity to waxoil inside the steel sill and remember the sill has an inner and outer section to it.
You might ask why have Jaguar chosen to do this. Some years ago manufacturers were directed to carry out drive by tests to measure the noise in decibels. This is called the drive by test. It includes the total package, body, engine, exhaust ,tyres and so on. An example of this is the under bonnet insulation. I am guessing that plastic engine covers ,wheel arch liners and the like all contribute to containing noise. So it could be that some benefit is gained by stuffing the sills full of foam.
I would not imagine that any manufacturer want their cars to live for ever, they are in the business of moving the metal. I do believe the design life is for ten years so if the addition of foam causes rot through at the end of this period then it is an opportunity to sell the next vehicle.
Looking at the age profile of the vehicles on E bay they have got it about right.
I would urge our XK brethren to be more concerned about metal corrosion than a bit of rash on a plastic sill and get those sills wax oiled
Oldtimer
I suspect that the construction of the XF in the sill area is identical to that of the S type and for that reason I would have the plastic over sills off and remove the foam insert. While at it,do not miss the opportunity to waxoil inside the steel sill and remember the sill has an inner and outer section to it.
You might ask why have Jaguar chosen to do this. Some years ago manufacturers were directed to carry out drive by tests to measure the noise in decibels. This is called the drive by test. It includes the total package, body, engine, exhaust ,tyres and so on. An example of this is the under bonnet insulation. I am guessing that plastic engine covers ,wheel arch liners and the like all contribute to containing noise. So it could be that some benefit is gained by stuffing the sills full of foam.
I would not imagine that any manufacturer want their cars to live for ever, they are in the business of moving the metal. I do believe the design life is for ten years so if the addition of foam causes rot through at the end of this period then it is an opportunity to sell the next vehicle.
Looking at the age profile of the vehicles on E bay they have got it about right.
I would urge our XK brethren to be more concerned about metal corrosion than a bit of rash on a plastic sill and get those sills wax oiled
Oldtimer
-
Brakebuster
- Posts:3145
- Joined:Tue Apr 18, 2006 1:17 pm
- Location:Gloucester UK
Re: Foam between outer and inner sills
Those of us more familiar with the S type model are only too well aware of corrosion beneath the plastic over sill. As conformation of this look at the list of S type Mot failures for sale on E bay together with copious amounts of copy and pictures on this subject on the S type section.
I suspect that the construction of the XF in the sill area is identical to that of the S type and for that reason I would have the plastic over sills off and remove the foam insert. While at it,do not miss the opportunity to waxoil inside the steel sill and remember the sill has an inner and outer section to it.
You might ask why have Jaguar chosen to do this. Some years ago manufacturers were directed to carry out drive by tests to measure the noise in decibels. This is called the drive by test. It includes the total package, body, engine, exhaust ,tyres and so on. An example of this is the under bonnet insulation. I am guessing that plastic engine covers ,wheel arch liners and the like all contribute to containing noise. So it could be that some benefit is gained by stuffing the sills full of foam.
I would not imagine that any manufacturer want their cars to live for ever, they are in the business of moving the metal. I do believe the design life is for ten years so if the addition of foam causes rot through at the end of this period then it is an opportunity to sell the next vehicle.
Looking at the age profile of the vehicles on E bay they have got it about right.
I would urge our XK brethren to be more concerned about metal corrosion than a bit of rash on a plastic sill and get those sills wax oiled
Oldtimer
i agree with the above , though not necessarily designed to ' rust ' it is inevitable for steel to do this, inclusion of foam is indeed for sound deadening, but it seriously limits the ability to fill the cavities with an aftermarket protective liquid, however, all modern cars are ' dipped ' before painting to completely fill all ' exposed ' cavities ' with a ' phosphate ' ( ? ) coating, though this wont reach these foam filled parts , which begs the question , are they dipped then foam filled or visa vera ?
being an avid scrap yard junkie , its more obvious now than ever before that there are no really rusty cars being scrapped ( compared to a yard full of old rovers, cortina's and vauxhall vivas ) , most are in there due to worn out drivetrain or emissions ,
either way , everything that is man made will eventually return to its natural state ( more or less ) and nothing lasts forever, no matter how much it costs to start with
BB
1989 5.3ltr V12 XJS Coupé FULLY RESTORED
2015 2.2TD Sportbrake in BRG and black leather
1994 3.2S XJ40 in Morocco Red with Doeskin interior
old cars
1999 4ltr Sovereign XJ8
2004 X-Type
2015 2.2TD Sportbrake in BRG and black leather
1994 3.2S XJ40 in Morocco Red with Doeskin interior
old cars
1999 4ltr Sovereign XJ8
2004 X-Type
-
ianoliver57

- Posts:261
- Joined:Fri Mar 14, 2014 11:19 pm
- Location:Tayvallich, Argyll.
Re: Foam between outer and inner sills
Thanks for the comments. Good advice to remove and have waxoil applied. I accept that cars do not rust these days to the same extent that they did, but, anything we can do to prolong good condition has got to be worth it. In my case, the car is 5 years old as of last December, but, with only 19K on the clock and imaculate inside and out, its got to be worth paying a bit to keep it in good condition. Now looking for a local facility to have it done.
Regards
Ian.
Regards
Ian.
2009 XJ8 Sovereign X358 Final Edition 4.2 V8.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Re: Foam between outer and inner sills
At our last breakfast get together at Kemble the subject of foam in XF sills came up . BB suggested that the foam was injected as a liquid after the sill was fitted . I've given this some thought and really cannot imagine what the situation is ! I guess I have used a similar expanding foam product in connect with building works. This stuff bonds to the surrounding surfaces superbly. Like wots- it to a blanket If indeed this is the case with XF sills how on earth does one remove the sill if it requires replacement due to damage.
So my question is :- Is it in fact a length of pre formed foam rubber insert - may-be, even similar to the inserts behind the plastic bumper cover, or is it a squirted in foam after assembly of the sill ?
If I had an XF Parts manual that would probably give us a clue.
I believe it is important to get a finite answer to this question because many XF's are approaching some degree of maturity and it would be sad to see them suffer the same corrosion problem as the S type
So my question is :- Is it in fact a length of pre formed foam rubber insert - may-be, even similar to the inserts behind the plastic bumper cover, or is it a squirted in foam after assembly of the sill ?
If I had an XF Parts manual that would probably give us a clue.
I believe it is important to get a finite answer to this question because many XF's are approaching some degree of maturity and it would be sad to see them suffer the same corrosion problem as the S type
Re: Foam between outer and inner sills
The issue has hit my previously owned 02 S-type. Its not been helped by the new owners lady having given the back ends of the sills a good thumping on some local speed bumps.
After fifteen years on the road, this years MOT flagged up advancing corrosion on the surface of the inner sills. An advisory note by the MOT tester suggests about a foot of new metal needs to be welded in before the next MOT test. I think it was Martec who said the rear ends of the sill cavities are left open at the back end. I wonder if that design aspect found its way into the XF?
I imagine the car was dipped and then expanding foam injected onto the protective dipped paint to form a chemically adhesive bond with the paint within the sills. I can`t imagine those sills would have been left as bare metal internally. A good void free bond between painted metal and the foam would be essential. Without that happening, there would always be a big chance that water ingress could occur between any air gaps left at the material interfaces.
Mike K
After fifteen years on the road, this years MOT flagged up advancing corrosion on the surface of the inner sills. An advisory note by the MOT tester suggests about a foot of new metal needs to be welded in before the next MOT test. I think it was Martec who said the rear ends of the sill cavities are left open at the back end. I wonder if that design aspect found its way into the XF?
I imagine the car was dipped and then expanding foam injected onto the protective dipped paint to form a chemically adhesive bond with the paint within the sills. I can`t imagine those sills would have been left as bare metal internally. A good void free bond between painted metal and the foam would be essential. Without that happening, there would always be a big chance that water ingress could occur between any air gaps left at the material interfaces.
Mike K
X350 Co-ordinator
2004 XJR
2004 XJR
-
Brakebuster
- Posts:3145
- Joined:Tue Apr 18, 2006 1:17 pm
- Location:Gloucester UK
Re: Foam between outer and inner sills
I imagine the car was dipped and then expanding foam injected onto the protective dipped paint to form a chemically adhesive bond with the paint within the sills. I can`t imagine those sills would have been left as bare metal internally. A good void free bond between painted metal and the foam would be essential. Without that happening, there would always be a big chance that water ingress could occur between any air gaps left at the material interfaces.
Mike K
my exact thoughts , it would be interesting to explore the exact process , and more importantly , to see if said ' foam ' is flame retardant , as local welding could be carried out if it is
modern cars use modern processes, and we must move with the times with regard to their repairs i suppose
BB
1989 5.3ltr V12 XJS Coupé FULLY RESTORED
2015 2.2TD Sportbrake in BRG and black leather
1994 3.2S XJ40 in Morocco Red with Doeskin interior
old cars
1999 4ltr Sovereign XJ8
2004 X-Type
2015 2.2TD Sportbrake in BRG and black leather
1994 3.2S XJ40 in Morocco Red with Doeskin interior
old cars
1999 4ltr Sovereign XJ8
2004 X-Type
-
ianoliver57

- Posts:261
- Joined:Fri Mar 14, 2014 11:19 pm
- Location:Tayvallich, Argyll.
Re: Foam between outer and inner sills
Interesting.
As far as I can see, the 'sponge' in the sill is not injected and stuck to the inner and outer sill. It is simply a loose bit of foam sponge type material which can be moved with ease. Not actually tried to pull it out yet, (assume it goes the full length) but it appears not to be stuck in. One thing I can confirm is that it is WET!!
Unless anyone comes up with a reason not to, I am going to try to remove it and have the area rust proofed.
Good idea??
Ian.
As far as I can see, the 'sponge' in the sill is not injected and stuck to the inner and outer sill. It is simply a loose bit of foam sponge type material which can be moved with ease. Not actually tried to pull it out yet, (assume it goes the full length) but it appears not to be stuck in. One thing I can confirm is that it is WET!!
Unless anyone comes up with a reason not to, I am going to try to remove it and have the area rust proofed.
Good idea??
Ian.
2009 XJ8 Sovereign X358 Final Edition 4.2 V8.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Previously
2004 S Type
2010 XF 3L petrol
2014 XF R-Sport
2010 XKR 5L
2011 XF S
2017 F Type 340
2019 XJ 3L V6
2021 XE R Dynamic P250 S
2021 F Type R Dynamic P450 AWD.
Re: Foam between outer and inner sills
The foam being wet is a good enough reason to remove it in my opinion. Some hot weather with the car left in the sun to dry the cavity out would appear to be the order of the day prior to inspection perhaps with an endoscope, followed by a good blast though with a wax oil type substance.
Few will possess an endoscope but they are surprisingly inexpensive via ebay. I think mine was about £30 and links via a USB cable to my laptop. Perhaps more versatile are the units which have their own display screen as part of the kit. That saves messing about with a laptop whilst under the car. I`ve tried that and the procedure is difficult and rather frustrating.
I`ve bought my last steel bodied car. I`m afraid I couldn`t get away from my S-type quick enough after its then fifteen year life on the road. I saw trouble ahead in the sill area and the last thing I wanted was to have to patch up a crumbling car. Everything else was in quite reasonable condition but I got a dose of the screaming hebe-jebies where sill structure was beginning to starting to show as the first signs of the end. The result was that I bought an aluminium bodied X350R which at thirteen years old displays an absolutely spotless corrosion free under body structure. Aluminium surely has to be the way forward. It may not eventually turn out to be the be all and end all of corrosion issues but it is certainly a significant step in the right direction.
That said of course, the subframes are always likely to be steel. Surface or indeed deeper corrosion will always be an issue there. I just wish car makers would produce longer lifed products in this respect. Sub-frames are never properly painted. I wish I had the disposable resources to have the frames out of the 350, stripped and sent off for blasting and a decent two pack primer and top coat applied.In twenty years or less though, the problem will probably not be an issue for me!
Believe me when I say I`m not being deliberately negative on corrosion issues but I just don`t have the time, patience, desire or finances to plough into ailing rotted out cars.
Mike K
Few will possess an endoscope but they are surprisingly inexpensive via ebay. I think mine was about £30 and links via a USB cable to my laptop. Perhaps more versatile are the units which have their own display screen as part of the kit. That saves messing about with a laptop whilst under the car. I`ve tried that and the procedure is difficult and rather frustrating.
I`ve bought my last steel bodied car. I`m afraid I couldn`t get away from my S-type quick enough after its then fifteen year life on the road. I saw trouble ahead in the sill area and the last thing I wanted was to have to patch up a crumbling car. Everything else was in quite reasonable condition but I got a dose of the screaming hebe-jebies where sill structure was beginning to starting to show as the first signs of the end. The result was that I bought an aluminium bodied X350R which at thirteen years old displays an absolutely spotless corrosion free under body structure. Aluminium surely has to be the way forward. It may not eventually turn out to be the be all and end all of corrosion issues but it is certainly a significant step in the right direction.
That said of course, the subframes are always likely to be steel. Surface or indeed deeper corrosion will always be an issue there. I just wish car makers would produce longer lifed products in this respect. Sub-frames are never properly painted. I wish I had the disposable resources to have the frames out of the 350, stripped and sent off for blasting and a decent two pack primer and top coat applied.In twenty years or less though, the problem will probably not be an issue for me!
Believe me when I say I`m not being deliberately negative on corrosion issues but I just don`t have the time, patience, desire or finances to plough into ailing rotted out cars.
Mike K
X350 Co-ordinator
2004 XJR
2004 XJR
Re: Foam between outer and inner sills
Ian,
I am pleased to read your thread above, I have suspected exactly what you have described as a preformed foam insert put in position during assembly. If the sill attachment resembles that of the S type there is a row of screws along the underneath bottom edge of the sill and a row of push in fasteners near the top of the sill which are released with a short sharp pull. With the sill cover off I guess you will find access holes which will allow a flexible waxoil lance in to do it's job. You may also find that a strengthening rib divides the metal sill through out its length creating an inner and outer section. I found that by taking the front plastic wheel arch liner out reveals an open end to the inner part of the sill which again allows the wax oil gun flexi lance to penetrate the full sill length.
You may be interested to know that the left hand and right hand windscreen drains pass through the inner wings and the water cascades down into the sill area. Bearing in mind that when salt is washed off the screen it passes down the drains and I'm sure does no good what so ever.
I use a Jack Sealy Wax oil gun which is supplied with two flexible lances ( Did cost £70.00 but worth every penny ) Although sold by Sealy it is a TEX gun the same as used in the factory. This gun of course needs an air supply from a compressor
I will be pleased to know what you find as I'm sure many of our readers will be
Oldtimer
PS Please bear in mind my experience is with regard to an S type and am guessing there are close similarities
I am pleased to read your thread above, I have suspected exactly what you have described as a preformed foam insert put in position during assembly. If the sill attachment resembles that of the S type there is a row of screws along the underneath bottom edge of the sill and a row of push in fasteners near the top of the sill which are released with a short sharp pull. With the sill cover off I guess you will find access holes which will allow a flexible waxoil lance in to do it's job. You may also find that a strengthening rib divides the metal sill through out its length creating an inner and outer section. I found that by taking the front plastic wheel arch liner out reveals an open end to the inner part of the sill which again allows the wax oil gun flexi lance to penetrate the full sill length.
You may be interested to know that the left hand and right hand windscreen drains pass through the inner wings and the water cascades down into the sill area. Bearing in mind that when salt is washed off the screen it passes down the drains and I'm sure does no good what so ever.
I use a Jack Sealy Wax oil gun which is supplied with two flexible lances ( Did cost £70.00 but worth every penny ) Although sold by Sealy it is a TEX gun the same as used in the factory. This gun of course needs an air supply from a compressor
I will be pleased to know what you find as I'm sure many of our readers will be
Oldtimer
PS Please bear in mind my experience is with regard to an S type and am guessing there are close similarities
Re: Foam between outer and inner sills
It is a very important point that Phil makes as regards the windscreen drains.
On Friday having been to Portsmouth Hospital, I called in on my old friends at Jagcare on the way home. The owner of the business, John and I were chatting about corrosion issues. He had just had to break bad news to an X-type owner that the sills on both sides of the car had virtually crumbled to nothing. Then he went on to discuss an S-type that was in an awful mess around the lower rear section behind the front wheel arch. He put that down to a blocked windscreen drain which as Phil says can easily block up. The front of the sill had disintegrated around where the back end of the front wing bolts. The damage had spread across the floor pan in front of the passenger foot well and to an area along the front of the sill area. John told me he could almost put his head inside the corroded area because the metal had corroded away.
AS Phil so wisely suggests, keep an eye for blocked windscreen drains.
Mike K.
On Friday having been to Portsmouth Hospital, I called in on my old friends at Jagcare on the way home. The owner of the business, John and I were chatting about corrosion issues. He had just had to break bad news to an X-type owner that the sills on both sides of the car had virtually crumbled to nothing. Then he went on to discuss an S-type that was in an awful mess around the lower rear section behind the front wheel arch. He put that down to a blocked windscreen drain which as Phil says can easily block up. The front of the sill had disintegrated around where the back end of the front wing bolts. The damage had spread across the floor pan in front of the passenger foot well and to an area along the front of the sill area. John told me he could almost put his head inside the corroded area because the metal had corroded away.
AS Phil so wisely suggests, keep an eye for blocked windscreen drains.
Mike K.
X350 Co-ordinator
2004 XJR
2004 XJR
Re: Foam between outer and inner sills
Mike ,
The whole object of the exercise is to prevent corrosion, not patch it up after the damage is done, that is too expensive and invariably too late. As you know I have a forty year old XJ which is a good example of how old iron car will survive with a few quid's worth of Wax oil.
Although aluminium has it's merits I'm not sure that it is the golden bullet. For a start aluminium hates salt, that is why the CAA forbids it's use for runway de icing. Also I have seen aircraft aluminium skin removed to expose rotten aluminium ribs. We won't go near the subject of inter crystalline corrosion.
In one of your previous threads you explained that you where preparing your car for the long haul, if that is the case I would start a regime of any corrosion work now despite the aluminium content. Waxoil costs £20 a gallon much cheaper than any repair
Just my thoughts on the subject
The whole object of the exercise is to prevent corrosion, not patch it up after the damage is done, that is too expensive and invariably too late. As you know I have a forty year old XJ which is a good example of how old iron car will survive with a few quid's worth of Wax oil.
Although aluminium has it's merits I'm not sure that it is the golden bullet. For a start aluminium hates salt, that is why the CAA forbids it's use for runway de icing. Also I have seen aircraft aluminium skin removed to expose rotten aluminium ribs. We won't go near the subject of inter crystalline corrosion.
In one of your previous threads you explained that you where preparing your car for the long haul, if that is the case I would start a regime of any corrosion work now despite the aluminium content. Waxoil costs £20 a gallon much cheaper than any repair
Just my thoughts on the subject
Re: Foam between outer and inner sills
The point is of course that prevention is worth a ton of repairs.
Indeed as an ex-CAA Licensed Engineer, pigs pee was by tradition the fluid that was sprayed on runways in an attempt to preventing iced landing strips. As you so rightly say Phil and to my knowledge also, that practice has now ceased...piggies and their effluent are high in salt.
There is not much one can do about internal inter-granular corrosion propagation. Seven thousand Series aluminium is particularly prone to that type of galvanic action. During our training the subject was covered in considerable detail. The classic unit shown for demonstration purposes was the angled wing joiner used in the low wing Piper Cherokee. That was effectively a seven series component that looked like a piece of angled I-beam about a foot long. It joined the two wings together along the line of the main wing spar. Thickness was about ten millimetres. It was subject to a mandatory annual inspection. What started out as ten mm thick, could expand in cross sectional area to about twenty mm. This was due to inter-granular action primarily caused by a very high zinc content which slept uneasily with the bauxite and copper content of the ali. You could see the layers of metal expanded to look like a pile of Autumn leaves. It was really quite alarming. The metal was a dark brown colour and the surface incredibly hard and brittle. If you dragged your knuckles across the corrosion, it could knife the skin off the back of your knuckles! Repair was by direct replacement of the affected part.
Coincidently, and quite by chance, I approved the a magazine pre-press PDF copy last night for Nigel on this very subject. This article will appear in the X350 pages in the March edition of the magazine.
As is frequently said, nothing lasts for ever and materials do have a nasty habit of returning to their natural state. Our task is to attempt to keep that reversion under some type of control.
I`d not considered applying wax oil type material in the sills of an aluminium car. Good idea, Phil. It can`t do any harm.
Mike
Indeed as an ex-CAA Licensed Engineer, pigs pee was by tradition the fluid that was sprayed on runways in an attempt to preventing iced landing strips. As you so rightly say Phil and to my knowledge also, that practice has now ceased...piggies and their effluent are high in salt.
There is not much one can do about internal inter-granular corrosion propagation. Seven thousand Series aluminium is particularly prone to that type of galvanic action. During our training the subject was covered in considerable detail. The classic unit shown for demonstration purposes was the angled wing joiner used in the low wing Piper Cherokee. That was effectively a seven series component that looked like a piece of angled I-beam about a foot long. It joined the two wings together along the line of the main wing spar. Thickness was about ten millimetres. It was subject to a mandatory annual inspection. What started out as ten mm thick, could expand in cross sectional area to about twenty mm. This was due to inter-granular action primarily caused by a very high zinc content which slept uneasily with the bauxite and copper content of the ali. You could see the layers of metal expanded to look like a pile of Autumn leaves. It was really quite alarming. The metal was a dark brown colour and the surface incredibly hard and brittle. If you dragged your knuckles across the corrosion, it could knife the skin off the back of your knuckles! Repair was by direct replacement of the affected part.
Coincidently, and quite by chance, I approved the a magazine pre-press PDF copy last night for Nigel on this very subject. This article will appear in the X350 pages in the March edition of the magazine.
As is frequently said, nothing lasts for ever and materials do have a nasty habit of returning to their natural state. Our task is to attempt to keep that reversion under some type of control.
I`d not considered applying wax oil type material in the sills of an aluminium car. Good idea, Phil. It can`t do any harm.
Mike
X350 Co-ordinator
2004 XJR
2004 XJR
Who is online
Users browsing this forum: No registered users and 1 guest